Process


Click here for
the process chart

01) 25 Tonnes-Electronic Arc Furnace plus AOD Refinery

02) Molten Steel into Mould Cooling Into Ingots

03) Ingots after Hot Rolling Process Into Round Bars

04) To peel the Bars to Remove Oxalates to make the surface smooth

05) Calculation and then Cutting of Round Bars

06) To Mark the Centering Points of Bars

07) To Heat the Bars under Temperature of 1150 degrees

08) To Drill the Heated Bars

09) Rapid Cooling Under Water Under Room Temperature

10) Annealing to Improve Microstructure, to Refine Grain sizes, to Modify Physical Prosperities,to Improve Machinability and to Make C Combined with Nickel to Avoid IGC Corrosion.

11) Pickling of Hollow Bars to Remove Surface Oxalate Residuals

12) Inspection on Hollow Bars

13) Lubrication of Hollow Bars to Make Surface Smooth

14) Cold Drawing plus Cold Pilgering

15) Pickling to Remove Oil and to Remove Surface Oxalate Residuals

16) Annealing & Solution of Pipes and Tubes

17) Straightening of Pipes and Tubes

18) Cutting

19) Pickling & Passivation

20) Inspection at Final Stage:
      a) Hydro Testing
      b) ET Testing
      c) UT Testing
      d) Mechanical, Technical & Hardness Test

21) Stenciling

22) Packing

23) Delivery